| Designation | HDT1200M |
| Alternative designation | HR900Y1180T-MS |
| Former designation | MS-W1200 |
| Standard | EN 10338 |
| Category | Martensitphasenstahl · Term explained |
| Density | 7.85 g/cm³ |
| Magnetism | ja |
| Equivalent grades | MS1200,MS-W1200,CR950Y1200T-MS,MART1200 |
| C | ≤ 0.25 |
| Si | ≤ 0.80 |
| Mn | ≤ 2.00 |
| P | ≤ 0.06 |
| S | ≤ 0.02 |
| Al | 0.02 – 2.00 |
| Cr+Mo | ≤ 1.20 |
| Nb+Ti | ≤ 0.20 |
| V | ≤ 0.22 |
| B | ≤ 0.01 |
| Yield strength Re (min) | 900 N/mm² |
| Tensile strength Rm | 1,200–1,400 N/mm² |
| Elongation at break A (min) | 3 % |
| Young's modulus | 210 GPa |